Nonmetallic Contamination on Copper Sample Testing, Bahrain

Enquiry:

After demolishing the loops of casting furnace 2, we noticed the presence of non-metallic contamination within the channel, which was the main cause of our furnace failure.

To identify the specific constituents responsible for this build-up, we would like to conduct a chemical analysis of our loop sample, including the contaminants.

Could you please reach out to labs that could potentially assist us with this?

PS: A picture of sample is attached for your reference.

Note sure if we need to do x ray diffraction or XRD to get the result.

Let us know if this is part of your scope or if you can provide a suggestion.


One of our highly proficient and ISO certified laboratory would be taking over this job.

Should you have any similar requisites, do drop us email and we shall revert instantly -> [email protected].