Enquiry:
After demolishing the loops of casting furnace 2, we noticed the presence of non-metallic contamination within the channel, which was the main cause of our furnace failure.
To identify the specific constituents responsible for this build-up, we would like to conduct a chemical analysis of our loop sample, including the contaminants.
Could you please reach out to labs that could potentially assist us with this?
PS: A picture of sample is attached for your reference.
Note sure if we need to do x ray diffraction or XRD to get the result.
Let us know if this is part of your scope or if you can provide a suggestion.
One of our highly proficient and ISO certified laboratory would be taking over this job.
Should you have any similar requisites, do drop us email and we shall revert instantly -> [email protected].